  • The key to this method is to keep porosity intergranular during pre-sintering, so that it can be removed subsequently by HIP treatment.
  • It was found that agglomerates of closely packed particles are helpful to reach that purpose, since they densify fully and leave only intergranular porosity.
  • Aluminium-based alloys may be sensitive to intergranular corrosion if there are layers of materials acting as anodes between the aluminium-rich crystals.
  • It is a purely empirical law attempting to describe ion flow ( mostly sodium and chloride ) in clean, consolidated sands, with varying intergranular porosity.
  • Components within s Brayton loops suffer from corrosion and erosion, specifically erosion in turbomachinery and recuperative heat exchanger components and intergranular corrosion and pitting in the piping.
  • The applied isostatic pressure provides additional driving force for densification by substantially increasing the atomic diffusion coefficients, which promotes additional viscous flow at or near grain boundaries and intergranular pores.
  • Working through ASTM International he was instrumental in standardizing intergranular corrosion tests, including the ferric sulfate-sulfuric acid test now called the " Streicher Test " in his honor.
  • Several methods have been used to control or minimize the intergranular corrosion of susceptible alloys, particularly of the annealing, quench-annealing or solution-quenching, has been used.
  • Intergranular corrosion is generally considered to be caused by the segregation of impurities at the grain boundaries or by enrichment or depletion of one of the alloying elements in the grain boundary areas.
  • They are formed as a glass, and then partially crystallized by heat treatment, producing both amorphous and crystalline phases so that crystalline grains are embedded within a non-crystalline intergranular phase.
  • While the intergranular failure problems noted above are sometimes severe, they are rarely the cause of major service failures ( in structural steels, for example ), as suitable safety margins are included in the designs.
  • An example of such texture, related to fractioned crystallization, is intergranular ( also known as intercumulus ) textures that develop wherever a mineral crystallizes later than the surrounding matrix, hence filling the left-over interstitial space.
  • The principle of effective stress, introduced by Karl Terzaghi, states that the effective stress " ? "'( i . e ., the average intergranular stress between solid particles ) may be calculated by a simple subtraction of the pore pressure from the total stress:
  • Perhaps the greater concern is that with the development of new technologies and materials with new and more extensive mechanical property requirements, and with the increasing impurity contents as a result of the increased recycling of materials, we may see intergranular failure in materials and situations not seen currently.
  • In the SiC / Al 2 O 3 system, for example, it is widely known and accepted that the addition of SiC particles to the Al 2 O 3 matrix results in a change of failure mechanism from intergranular ( between grains ) to intragranular ( within grains ) fracture.
  • Putting aside some of the well known facts about deposit phosphorus vs various properties, i . e . hardness or corrosion resistance that we will cover a bit later, deposits with a high degree of amorphous composition are free of grain boundaries, which typically act as sites for intergranular corrosion commonly encountered in crystalline deposits.
  • Furthermore, results indicate that microscopic pores in sintered ceramic nanomaterials, mainly trapped at the junctions of microcrystalline grains, cause light to scatter and prevented true transparency . it has been observed that the total volume fraction of these nanoscale pores ( both intergranular and intragranular porosity ) must be less than 1 % for high-quality optical transmission.
  • High-strength aluminium alloys such as the Duralumin-type alloys ( Al-Cu ) which depend upon precipitated phases for strengthening are susceptible to intergranular corrosion following sensitization at temperatures of about 120 �C . Nickel-rich alloys such as Inconel 600 and Incoloy 800 show similar susceptibility . steam generators, or as a result of subsequent welding of the formed structure.